{"_buckets": {"deposit": "05edf62f-0608-4645-ba53-cfca87d370ca"}, "_deposit": {"id": "20812", "owners": [], "pid": {"revision_id": 0, "type": "depid", "value": "20812"}, "status": "published"}, "_oai": {"id": "oai:nagoya.repo.nii.ac.jp:00020812", "sets": ["322"]}, "author_link": ["60214", "60215", "60216", "60217", "60218", "60219"], "item_10_alternative_title_19": {"attribute_name": "その他のタイトル", "attribute_value_mlt": [{"subitem_alternative_title": "EFFECT OF HEATING AND COOLING PROCESS ASSUMING FIRE OF STEEL BRIDGES ON CHARACTERISTICS OF WELDED JOINTS OF STRUCTURAL STEEL", "subitem_alternative_title_language": "en"}]}, "item_10_biblio_info_6": {"attribute_name": "書誌情報", "attribute_value_mlt": [{"bibliographicIssueDates": {"bibliographicIssueDate": "2014-12", "bibliographicIssueDateType": "Issued"}, "bibliographicIssueNumber": "84", "bibliographicPageEnd": "78", "bibliographicPageStart": "67", "bibliographicVolumeNumber": "21", "bibliographic_titles": [{"bibliographic_title": "鋼構造論文集", "bibliographic_titleLang": "ja"}]}]}, "item_10_description_4": {"attribute_name": "抄録", "attribute_value_mlt": [{"subitem_description": "For investigating the effect of heating and cooling process assuming fire of steel bridges on characteristics of welded joints of structural steel members, a series of experiments were carried out. The heating under transformation point did not affect the joint performance regardless of cooling process. The heating over transformation point caused the softening or the hardening according to cooling rate. The degree of them was larger in the base metal rather than in the weld metal because the amount of carbon in the base metal was more than that in the weld metal. Furthermore, the change of microstructure of base metal made by TMC process was more sensitive compared with that of weld metal.", "subitem_description_language": "en", "subitem_description_type": "Abstract"}]}, "item_10_identifier_60": {"attribute_name": "URI", "attribute_value_mlt": [{"subitem_identifier_type": "HDL", "subitem_identifier_uri": "http://hdl.handle.net/2237/22942"}]}, "item_10_publisher_32": {"attribute_name": "出版者", "attribute_value_mlt": [{"subitem_publisher": "日本鋼構造協会", "subitem_publisher_language": "ja"}]}, "item_10_select_15": {"attribute_name": "著者版フラグ", "attribute_value_mlt": [{"subitem_select_item": "author"}]}, "item_10_source_id_7": {"attribute_name": "ISSN", "attribute_value_mlt": [{"subitem_source_identifier": "1880-9928", "subitem_source_identifier_type": "PISSN"}]}, "item_1615787544753": {"attribute_name": "出版タイプ", "attribute_value_mlt": [{"subitem_version_resource": "http://purl.org/coar/version/c_ab4af688f83e57aa", "subitem_version_type": "AM"}]}, "item_access_right": {"attribute_name": "アクセス権", "attribute_value_mlt": [{"subitem_access_right": "open access", "subitem_access_right_uri": "http://purl.org/coar/access_right/c_abf2"}]}, "item_creator": {"attribute_name": "著者", "attribute_type": "creator", "attribute_value_mlt": [{"creatorNames": [{"creatorName": "廣畑, 幹人", "creatorNameLang": "ja"}], "nameIdentifiers": [{"nameIdentifier": "60214", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "北根, 安雄", "creatorNameLang": "ja"}], "nameIdentifiers": [{"nameIdentifier": "60215", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "伊藤, 義人", "creatorNameLang": "ja"}], "nameIdentifiers": [{"nameIdentifier": "60216", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "HIROHATA, Mikihito", "creatorNameLang": "en"}], "nameIdentifiers": [{"nameIdentifier": "60217", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "KITANE, Yasuo", "creatorNameLang": "en"}], "nameIdentifiers": [{"nameIdentifier": "60218", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "ITOH, Yoshito", "creatorNameLang": "en"}], "nameIdentifiers": [{"nameIdentifier": "60219", "nameIdentifierScheme": "WEKO"}]}]}, "item_files": {"attribute_name": "ファイル情報", "attribute_type": "file", "attribute_value_mlt": [{"accessrole": "open_date", "date": [{"dateType": "Available", "dateValue": "2018-02-21"}], "displaytype": "detail", "download_preview_message": "", "file_order": 0, "filename": "1-6.pdf", "filesize": [{"value": "1.3 MB"}], "format": "application/pdf", "future_date_message": "", "is_thumbnail": false, "licensetype": "license_note", "mimetype": "application/pdf", "size": 1300000.0, "url": {"label": "1-6.pdf", "objectType": "fulltext", "url": "https://nagoya.repo.nii.ac.jp/record/20812/files/1-6.pdf"}, "version_id": "b783faab-58a0-4a0c-b2c4-00af84098de4"}]}, "item_keyword": {"attribute_name": "キーワード", "attribute_value_mlt": [{"subitem_subject": "鋼橋", "subitem_subject_scheme": "Other"}, {"subitem_subject": "火災", "subitem_subject_scheme": "Other"}, {"subitem_subject": "溶接継手", "subitem_subject_scheme": "Other"}, {"subitem_subject": "構造用鋼", "subitem_subject_scheme": "Other"}, {"subitem_subject": "TMCP鋼", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Steel bridge", "subitem_subject_scheme": "Other"}, {"subitem_subject": "fire", "subitem_subject_scheme": "Other"}, {"subitem_subject": "welded joints", "subitem_subject_scheme": "Other"}, {"subitem_subject": "structural steel", "subitem_subject_scheme": "Other"}, {"subitem_subject": "TMCP steel", "subitem_subject_scheme": "Other"}]}, "item_language": {"attribute_name": "言語", "attribute_value_mlt": [{"subitem_language": "jpn"}]}, "item_resource_type": {"attribute_name": "資源タイプ", "attribute_value_mlt": [{"resourcetype": "journal article", "resourceuri": "http://purl.org/coar/resource_type/c_6501"}]}, "item_title": "鋼橋の火災を想定した加熱および冷却過程が構造用鋼の溶接継手特性に及ぼす影響", "item_titles": {"attribute_name": "タイトル", "attribute_value_mlt": [{"subitem_title": "鋼橋の火災を想定した加熱および冷却過程が構造用鋼の溶接継手特性に及ぼす影響", "subitem_title_language": "ja"}]}, "item_type_id": "10", "owner": "1", "path": ["322"], "permalink_uri": "http://hdl.handle.net/2237/22942", "pubdate": {"attribute_name": "PubDate", "attribute_value": "2015-08-04"}, "publish_date": "2015-08-04", "publish_status": "0", "recid": "20812", "relation": {}, "relation_version_is_last": true, "title": ["鋼橋の火災を想定した加熱および冷却過程が構造用鋼の溶接継手特性に及ぼす影響"], "weko_shared_id": -1}
鋼橋の火災を想定した加熱および冷却過程が構造用鋼の溶接継手特性に及ぼす影響
http://hdl.handle.net/2237/22942
http://hdl.handle.net/2237/22942ce13334a-4249-4ede-83f5-1fec599d864f
名前 / ファイル | ライセンス | アクション |
---|---|---|
1-6.pdf (1.3 MB)
|
|
Item type | 学術雑誌論文 / Journal Article(1) | |||||
---|---|---|---|---|---|---|
公開日 | 2015-08-04 | |||||
タイトル | ||||||
タイトル | 鋼橋の火災を想定した加熱および冷却過程が構造用鋼の溶接継手特性に及ぼす影響 | |||||
言語 | ja | |||||
その他のタイトル | ||||||
その他のタイトル | EFFECT OF HEATING AND COOLING PROCESS ASSUMING FIRE OF STEEL BRIDGES ON CHARACTERISTICS OF WELDED JOINTS OF STRUCTURAL STEEL | |||||
言語 | en | |||||
著者 |
廣畑, 幹人
× 廣畑, 幹人× 北根, 安雄× 伊藤, 義人× HIROHATA, Mikihito× KITANE, Yasuo× ITOH, Yoshito |
|||||
アクセス権 | ||||||
アクセス権 | open access | |||||
アクセス権URI | http://purl.org/coar/access_right/c_abf2 | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | 鋼橋 | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | 火災 | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | 溶接継手 | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | 構造用鋼 | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | TMCP鋼 | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | Steel bridge | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | fire | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | welded joints | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | structural steel | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | TMCP steel | |||||
抄録 | ||||||
内容記述 | For investigating the effect of heating and cooling process assuming fire of steel bridges on characteristics of welded joints of structural steel members, a series of experiments were carried out. The heating under transformation point did not affect the joint performance regardless of cooling process. The heating over transformation point caused the softening or the hardening according to cooling rate. The degree of them was larger in the base metal rather than in the weld metal because the amount of carbon in the base metal was more than that in the weld metal. Furthermore, the change of microstructure of base metal made by TMC process was more sensitive compared with that of weld metal. | |||||
言語 | en | |||||
内容記述タイプ | Abstract | |||||
出版者 | ||||||
言語 | ja | |||||
出版者 | 日本鋼構造協会 | |||||
言語 | ||||||
言語 | jpn | |||||
資源タイプ | ||||||
資源タイプresource | http://purl.org/coar/resource_type/c_6501 | |||||
タイプ | journal article | |||||
出版タイプ | ||||||
出版タイプ | AM | |||||
出版タイプResource | http://purl.org/coar/version/c_ab4af688f83e57aa | |||||
ISSN | ||||||
収録物識別子タイプ | PISSN | |||||
収録物識別子 | 1880-9928 | |||||
書誌情報 |
ja : 鋼構造論文集 巻 21, 号 84, p. 67-78, 発行日 2014-12 |
|||||
著者版フラグ | ||||||
値 | author | |||||
URI | ||||||
識別子 | http://hdl.handle.net/2237/22942 | |||||
識別子タイプ | HDL |